Failure Analysis of Weld Cracking in External Cold Water Pipeline of Condenser in Converter Station
1 State Grid Hunan Electric Power Company Limited Research Institute, Changsha 410007, China
2 China Electric Power Research Institute, Beijing, 100192, China
3 State Grid Zhejiang Electric Power Research Institute, Hangzhou, 410007, China
* Corresponding author: 279091498@qq.com
The cause of weld cracking in external cold water pipeline of condenser in a ±800kV converter station were analyzed by macro inspection, chemical composition analysis, hardness test, microstructure inspection, scanning electron microscopy and energy spectrum test methods.The results show that the main reason for the cracks is that the material and manufacturing process are not qualified, and the welding process is not good. Corresponding control measures are put forward to avoid similar failures from happening again.
© The Authors, published by EDP Sciences, 2020
This is an Open Access article distributed under the terms of the Creative Commons Attribution License 4.0, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.
Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.
Initial download of the metrics may take a while.